View Single Post
  #16   Spotlight this post!  
Unread 22-07-2013, 14:08
KrazyCarl92's Avatar
KrazyCarl92 KrazyCarl92 is offline
Registered User
AKA: Carl Springli
FRC #5811 (The BONDS)(EWCP)
Team Role: Mentor
 
Join Date: Jan 2010
Rookie Year: 2010
Location: Dayton, OH
Posts: 519
KrazyCarl92 has a reputation beyond reputeKrazyCarl92 has a reputation beyond reputeKrazyCarl92 has a reputation beyond reputeKrazyCarl92 has a reputation beyond reputeKrazyCarl92 has a reputation beyond reputeKrazyCarl92 has a reputation beyond reputeKrazyCarl92 has a reputation beyond reputeKrazyCarl92 has a reputation beyond reputeKrazyCarl92 has a reputation beyond reputeKrazyCarl92 has a reputation beyond reputeKrazyCarl92 has a reputation beyond repute
Re: pic: 20's IRI Carnage

Quote:
Originally Posted by Cory View Post
7075 is not the problem. We have used it since 2007 with zero failures.

Most common grades of stainless are actually substantially weaker than 7075, unless AM is using a prehard grade (13-8, 15-5, 17-4) or 410/416
Do you mean 7075 is stronger per unit weight, or stronger for a given cross-sectional area?