AlecMataloni has a reputation beyond reputeAlecMataloni has a reputation beyond reputeAlecMataloni has a reputation beyond reputeAlecMataloni has a reputation beyond reputeAlecMataloni has a reputation beyond reputeAlecMataloni has a reputation beyond reputeAlecMataloni has a reputation beyond reputeAlecMataloni has a reputation beyond reputeAlecMataloni has a reputation beyond reputeAlecMataloni has a reputation beyond reputeAlecMataloni has a reputation beyond repute
Re: Killer Bees - 2014

So, what's the standard bend radius on the .050 sheet you guys use? I've read that 6061-T6 bends poorly/ cracks below a bend radius of double the material thickness. Is this the rule of thumb you follow?