Laser would only take about 30 minutes to cut all that, and it would not have any draft. But, you would have to deburr.
Nice job looks like you have a lot of welding to do. maybe think about using 3/16 pop rivets in your design next time with an air rivet gun.
Bend flanges on the parts to rivet into.
The welding will weaken the aluminum by taking the hardeness down to T Zero at welds unless you have the frame reaged.
|