Re: Banebot 56mm gearbox - homebrew hardening?
Would a homebrew hardening of the plate be of use in helping this problem? Heating it to red-hot and tossing it into a bucket of cold water seems like a fun experiment. Into potentially explosive oil could be even more exciting (just kidding, this could/would be very dangerous). http://www.efunda.com/processes/heat...ing/direct.cfm
__________________
There's a fine line between fishing and just standing on the shore like an idiot. - Stephen Wright 
________________________________________
2007 UTC Regional - Finalists (thanks 25 & 176)
Last edited by flightofone : 29-01-2007 at 19:53.
|