sanddrag has a reputation beyond reputesanddrag has a reputation beyond reputesanddrag has a reputation beyond reputesanddrag has a reputation beyond reputesanddrag has a reputation beyond reputesanddrag has a reputation beyond reputesanddrag has a reputation beyond reputesanddrag has a reputation beyond reputesanddrag has a reputation beyond reputesanddrag has a reputation beyond reputesanddrag has a reputation beyond repute
Re: Designing Anodized Parts

A machinist I know said for a traditional basic anodizing, the dimension added (outside the existing material) is so negligable .0002-.0003" that it doesn't need to be considered for most bearing press fits. If you are getting into hard anodizing, it is possible you could add a thou or two, and then it would need to be considered.

Last edited by sanddrag : 23-04-2007 at 23:05.