Cory has a reputation beyond reputeCory has a reputation beyond reputeCory has a reputation beyond reputeCory has a reputation beyond reputeCory has a reputation beyond reputeCory has a reputation beyond reputeCory has a reputation beyond reputeCory has a reputation beyond reputeCory has a reputation beyond reputeCory has a reputation beyond reputeCory has a reputation beyond repute
Send a message via AIM to Cory
Re: pic: A new End Mill from McMaster

Next time you buy some new end mills, go for something without the TiN coating.

TiN is not a good coating for non ferrous metals. You'd do much better with TiCN. Absolutely avoid TiAlN or AlTiN for aluminum.

You should try some 3 flute carbide variable helix ZrN coated end mills. You can get them pretty cheap, and they cut like a dream on Al.