Quote:
Originally Posted by rc_cola1323
UHMW is a harder plastic than delrin. Our Mcmaster Carr ones only wore 3/16th's and we used them for almost 2 years.
|
not in all cases. standard uhmw is around 66 shore D while Delrin is around 86 shore D
Since these are both plastics which can contain glass filling, other materials, recycled plastic it is not wise to make generalizations about materials. Especally in this case where you didn't state the exact material which these are molded and the exact type of delrin they used.
On another note, I am not sure that hardness is the correct measure for effective chain tensioners. I would think it has to do with the lubricity of the material and the ductility. While hardness probably comes into play (ie why gum rubber wouldn't be a good tensioner) It is not the only (or possibly the main one) which needs to be considered.