Thread: Steel Frame
View Single Post
  #13   Spotlight this post!  
Unread 17-01-2010, 18:03
mark johnson's Avatar
mark johnson mark johnson is offline
Registered User
FRC #3175 (knight vision)
Team Role: Mentor
 
Join Date: Mar 2005
Rookie Year: 2000
Location: clinton twp michigan
Posts: 71
mark johnson has much to be proud ofmark johnson has much to be proud ofmark johnson has much to be proud ofmark johnson has much to be proud ofmark johnson has much to be proud ofmark johnson has much to be proud ofmark johnson has much to be proud ofmark johnson has much to be proud ofmark johnson has much to be proud of
Re: Steel Frame

Quote:
Originally Posted by silv940 View Post
I don't understand the question
Normalizing in simple terms is post heating the weld to relieve stress from the weld process. Actually when you weld chrome moly tube you should pre and post heat the weld joint but i know alot of chassis builders that do not and have no problem. Another way you can normalize the frame is to totally finish the frame , drill tiny holes by each weld joint and have the whole frame heated in a oven , this will take out all stresses built up by the welding process.