Re: Banebot 56mm gearbox - double D - RELOADED
I know the best solution to the carrier plate is a new properly heat treated replacement, but could brazing the shaft and carrier together overcome the problem? This might help if the spacing issue agravates the carrier wipe out.
A good 16% silver brazing rod and the proper flux should penetrate well. What woud taking the carrier and shaft up to 1300 - 1400 F do to the hardness? Water quench after? |
| Thread Tools | |
| Display Modes | Rate This Thread |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Banebot 56mm gearbox - double D related | Joe Johnson | Motors | 78 | 31-01-2007 23:55 |
| small banebot motor with 64:1 gearbox | burkey_turkey | Motors | 16 | 29-01-2007 01:48 |
| Banebot Gearbox | chris31 | Technical Discussion | 45 | 15-01-2007 17:56 |
| Attempting to Cut BaneBot 56mm Shaft | edthegeek | Motors | 6 | 15-01-2007 08:51 |
| 56mm BaneBot Gearbox 15tooth sprockets. Where to buy more? | VEN | Technical Discussion | 4 | 11-01-2007 14:45 |